Makonat - Machine Plaster
Physical Form |
white powder |
Plaster/Water Ratio |
10 Kg for 5.5-6 Lt Water |
Usage Time |
130-180 minutes |
Freezing Time |
250-300 minutes |
Consumption Amount |
9.0-9.5 Kg/m³ (every 1 cm thickness) |
Compressive Strength |
2.5 N/mm² (4x4x16 blocks) |
Flexural Strength |
1.0 N/mm² (4x4x16 blocks) |
Dry Unit Weight |
730-800 Kg/m³ |
Response to Fire |
A1 (According to TS EN 13279 – 1) |
Related Standard |
13279-1.2 (Type B4, Machine Applied Spray)
|
SURFACE AND ENVIRONMENT DURING THE APPLICATION
-It should be free from dirty materials such as dust, oil, paint. -Extremely dry, hot and highly absorbent surfaces should be moistened with water. -The surface of the ceilings should be roughened before applying the plaster or primed with a material that allows the mortar to stick to the surface to the surface. there should not be air flow or circulation in the environment during the application.
APPLICATION
It is prepared in the plaster machine with the enough proportion of plaster/water (5.5-6 lt water/10 kg makonat). The mortar is sprayed onto the surface by machine. According to the smoothness of the surface, the application thickness is determined with the help of slabs. The plaster applied to the surface is corrected with the help of a gauge. When the surface starts to harden, smoothing is done with a steel trowel. When the surface reaches a consistency that will not collapse when lightly pressed with a finger, trifiling is done. After the trifiling process, the surface will be ready for painting by polishing again with a steel trowel for painting by polishing again with a steel trowel.
PACKAGING
Polypropylene bag 35 kg (+- 2%)
STORAGE
Maximum 15 bags should be stockpield on top of each other in a dry place and the bags should be stored in such a way that they do not come into contact with the ground and are protected from moisture and condensation. It should be used within 6 months from the date of manufacture.