Yaponat - Adhesive Plaster
Physical Form |
white powder |
Plaster/Water Proportion |
10 Kg for 5.5 Lt Water |
Usage Time |
60-90 minutes |
Freezing Time |
140-180 minutes |
Consumption Amount |
5 Kg/m² (per 1 mm thickness) |
Compressive Strength |
6.0 N/mm² (4x4x16 blocks) |
Flexural Strength |
1.0 N/mm² (4x4x16 blocks) |
Dry Unit Weight |
680-720 Kg/m³ |
Fire Response |
A1 (TS EN 13279-1) |
Related Standard |
TSE EN 14496 |
SURFACE AND ENVIRONMENT DURING THE APPLICATION
-It must be clean and free from materials such as dust, oil, paint. -Extremely dry, hot and highly absorbent surfaces should be moistened with water. -There should not be air flow or circulation in the environment during the application.
-The temperature of the environment should be between +5 C and +40 C.
APPLICATION
5 – 5.5 liters of clean water is poured into the mortarboard in order to mix. 10 kg of YAPONAT is poured into it by sprinkling. It is awaited for 2-3 minutes to make sure the plaster absorbs the water. It is mixed with a mixer or trowel until a homogeneous mixture is obtained. The prepared mortar is applied to the surface to be applied yerine by applying as groups of it to the intervals. After the bonding process, the smoothness of the pasted surface should be checked.
PACKAGING
Polypropylene bag 30 kg (+- 2%)
STORAGE
Maximum 20 bags should be stockpiled on top of each other in a dry place, and the bags should be stored in such a way that they do not come into contact with the ground and are protected from moisture and condensation. It should be used within 9 months from the date of manufacture.